Aluminum Alloys for CNC Machining

cnc milling

Start with 6061-T6 for general machined parts, consider 6082-T6 for structural work, and evaluate 7075 when the design calls for higher strength. The right choice also depends on the temper, stock form, exposure and finish.

For parts made to your drawing, see our aluminum CNC machining service.

6061 vs 6082 vs 7075 aluminum

General machining

6061-T6

Choose it for. General machining and anodizing.

Material at a glance
  • Alloy familyAl–Mg–Si
  • Stock and temperT6 bar or extrusion, T651 plate where specified

A starting point for brackets, fixtures and housings. It balances strength, corrosion resistance and machinability and takes anodizing well. If the part is mostly a visible extrusion, compare 6063. See our 6061-T6 machining guide. T6 describes a solution heat-treated and artificially aged condition. For plate with substantial stock removal, consider a stress-relieved temper such as T651 and agree the stock specification.

Before specifying
Verify stock form, finish and distortion risk after heavy material removal.
Structural parts

6082-T6

Choose it for. Structural mounts and profiles.

Material at a glance
  • Alloy familyAl–Mg–Si–Mn
  • Stock and temperT6 structural extrusion or plate, subject to stock specification

Consider it for loaded mounts and structural profiles. Hydro reports higher strength than 6061 for its extrusion products. Check the properties for the exact thickness and stock form before approving a substitution. Hydro also notes that thin, complex extrusions can be harder to produce in 6082-T6, so verify availability in the required section.

Before specifying
Compare minimum properties for the actual section. Thin extrusions can limit T6 availability.
Higher strength

7075-T6 / T651

Choose it for. High strength in a compact section.

Material at a glance
  • Alloy familyAl–Zn–Mg–Cu
  • Stock and temperT6 bar or T651 plate, with overaged alternatives by product form

Consider 7075 for compact, highly loaded parts where strength is a priority. Check corrosion exposure and the finish requirement early. Use the properties for the specified temper and stock form when checking the design. T651 includes stress relief by stretching. If stress-corrosion resistance governs, compare overaged tempers such as T73 or T7351 where available for the specified product form.

Before specifying
Check corrosion exposure, finish and whether an overaged temper fits the design.

When another grade fits better

Extruded profiles and visible trim

6063

Choose it for. Decorative anodizing and visible profiles.

Material at a glance
  • Alloy familyAl–Mg–Si
  • Stock and temperT5 or T6 extrusion

6063-T5 and T6 are common extrusion tempers. Hydro rates 6063 ahead of 6082 for decorative anodizing and behind it for tensile strength and machinability. Compare the temper and wall thickness if the profile carries load.

Before specifying
Check wall thickness and temper where the profile carries load.
Bent sheet panels and covers

5052

Choose it for. Bending and corrosion resistance.

Material at a glance
  • Alloy familyAl–Mg
  • Stock and temperH32 sheet for formed panels

5052-H32 is strain hardened and stabilized. Its corrosion resistance and formability suit parts that need bends. Check the bend radius for the sheet thickness and temper. For deep pockets machined from solid stock, compare 6061 plate.

Before specifying
Verify bend radius against sheet thickness, temper and grain direction.
Parts with fatigue and strength requirements

2024

Choose it for. Machined parts with strength and fatigue requirements.

Material at a glance
  • Alloy familyAl–Cu–Mg
  • Stock and temperT3 sheet or T351 plate

2024-T3 sheet and T351 plate are distinct product choices. The alloy machines well in common heat-treated tempers, but bare 2024 has relatively poor general corrosion resistance. Specify protection for the service environment and check the applicable stock data.

Before specifying
Specify corrosion protection and check whether the design requires bare or clad stock.
Repetitive turning from bar

2011

Choose it for. Repetitive CNC turning.

Material at a glance
  • Alloy familyAl–Cu free-machining alloy
  • Stock and temperT3 or T8 rod and bar

2011 is a free-machining alloy suited to automatic lathes, where short chips help evacuation. It can contain lead, so verify the actual bar specification against any customer material restrictions before approving it.

Before specifying
Confirm the stock chemistry against customer restrictions and check corrosion and finish requirements.
Low-load parts that need forming

1100

Choose it for. Low-load formed parts.

Material at a glance
  • Alloy familyCommercially pure aluminum
  • Stock and temperO or H14 sheet, depending on the forming requirement

Commercially pure 1100 offers good formability and corrosion resistance with relatively low strength. Soft stock can produce gummy chips. Check whether the part needs a harder temper or a different grade for machining or load capacity.

Before specifying
O temper favors forming. Check strength and chip control if machining follows.
Formed parts that need more strength than 1100

3003

Choose it for. Formed parts needing more strength than 1100.

Material at a glance
  • Alloy familyAl–Mn
  • Stock and temperO or H14 sheet, depending on the forming requirement

Manganese gives 3003 more strength than 1100 while retaining useful formability. Compare the sheet temper and bend requirements. Like 1100, softer conditions can produce gummy chips during machining.

Before specifying
Check bend requirements and chip control for the specified temper.

What to specify before machining

Alloy, temper and stock form. Call out the required designation and whether the part starts from plate, bar, sheet or extrusion. T6 is a heat-treated condition. T651 also includes stress relief by stretching. Confirm the exact material specification before approving a substitute.

Finish and exposure. Note the service environment, cosmetic faces, color reference and areas to mask. For parts assembled side by side, confirm the appearance with a sample of the intended alloy and finish. The blue anodized housing example explains how to specify shade, coating thickness and masked surfaces.

Dimensions after finishing. Mark fits and other critical features on the drawing. Say which dimensions must be verified after finishing, and include any inspection or material documentation requirements when you request a machining quote.

Drawings vs 3D files

Supplier data for alloy selection

Start with the datasheet for the stock you will buy. Use Hydro’s extrusion data for profiles, and Kaiser’s rod and bar data for parts turned from solid bar. For sheet or plate, use the supplier’s data for that product form.

Check the exact alloy, temper, thickness range and test direction. Compare the specified minimum yield strength, tensile strength and elongation for the actual stock. Use typical values for screening, and check the material specification for the requirements that apply to your order. If appearance matters, agree on a finish sample made from the intended stock.

Hydro 6061 · Hydro 6082 · Hydro 6063 · Kaiser 2024 · Kaiser 7075 · Kaiser stock data for 1100, 2011, 3003 and 5052 · Kaiser 2011 rod and bar

Aluminum alloy selection questions

Is 6082-T6 interchangeable with 6061-T6?

Check the drawing and ask for approval before substituting. Compare the specified minimum properties for the stock form and thickness, as well as the finish and any welding requirements.

When is 7075 worth considering over 6061?

Compare 7075 when the design needs higher strength within a limited part size or weight. Include corrosion exposure, finish requirements and the available temper in the decision.

Can different grades match after anodizing?

The alloy, stock and surface preparation can change the appearance. If adjacent parts must match, agree a sample using the intended stock and finish.

What is the difference between T6 and T651?

T6 means the alloy was solution heat treated and artificially aged. T651 also includes stress relief by stretching. For a part machined from thick plate, specify the required temper and confirm the material standard with the supplier.

Should I choose 5052 or 6061 for a bent panel?

Start by comparing 5052-H32 sheet for a panel that needs bending. For a part with deep pockets machined from solid stock, compare 6061 plate. Check the minimum bend radius for the actual sheet thickness, temper and grain direction.

Should I choose 6063 or 6082 for an extrusion?

Compare 6063 when visible surface quality and decorative anodizing are priorities. Consider 6082 when the profile carries structural loads. Check the minimum properties and temper availability for the actual profile and wall thickness.

What information should go on the drawing for an alloy substitution?

State the required alloy, temper, material standard and stock form. If an alternative is allowed, document the approval and check minimum mechanical properties, corrosion exposure, joining and finish requirements before release.